Film thickness, morphology and orientation could be effectively controlled by adjusting crystallization time and times. The best molar composition of Ti/ Si, H2O/ Si and TPAOH/ Si in mother liquid was 0.02,250 and 0.35.

  • 改变晶化时间和次数可有效调节膜厚度、形貌和取向;母液中最优Ti/Si、H2O/Si和TPAOH/Si摩尔比为0.02、250和0.35。