Dewax are first done by boiling and second by warm water.
退蜡沸水退蜡,二次退蜡用温水.
The dewax rate is controlled by the diffusion of paraffin wax in poly propylene.
热脱蜡的动力学控制步骤为石蜡在聚丙烯中的扩散过程.