Slag, blowholes, and paint on unfused regions were observed at the welded junctions.
在焊接处看到了夹渣, 气孔及未熔透区的油漆.
This indicated that the fracture had initiated at the unfused butt weld in the longitudinal stiffener.
研究表明裂纹是从纵向加劲助未熔透的对接焊缝中起始的.